Manufacturer of Rubber foam insulation sheet and pipe:
1.low thermal conductivity
2.full-closed structure
3.CE, SGS, RoHSDistinctive advantages:
• Closed structure can effectively prevent thermal conduction.
• Thermal conductivity :0.034W/m
• k while 0
• High heat emission coefficient of surface, up to 9W/m2k
• Excellent anti-steam permeated ability; moisture resistance 10,000 (DIN 52615); "built-in" steam-proof coating; the insulation board is insulating layer and moisture-proof coating as well.
• Excellent fireproofing; oxygen index is above 40.
• Easy for installation.
• No CFC, HFC, HCFC or other materials containing fluorine, also no formaldehyde, dust or fiber.
Product specifications:
Rubber plastic board (1m wide)
Thickness
6mm
9mm
15mm
18mm
20mm
25mm
28mm
30mm
m/pcs
20m
20m
10m
10m
10m
8m
8m
8m
It can be ordered to produce if there is big demand of board with thickness of 13mm, 18mm, 23mm or 28mm.
Rubber plastic pipe
ID: 6-108mm thickness 9-30mm length:1.8 1.9 2.0m
Technical Specifications of NBR/PVC:
Item
Unit
Specification
Standard
Density
Kg/m³
≤95
GB/T6343
Flammability
Oxygen index
%
≥32
GB/T2406
SDR
——
≤75
GB/T8627
Conductivity factor
Average temperature
-20°C
0°C
40°C
W/(m.k)
≤0.031
≤0.034
≤0.036
GB/T10294
Watervapor permeability
Coefficient
g/(m.s.pa)
≤2.8*10-11
GB/T17146-1997
Factor
——
≥7.0*10³
Water absorption ratio in vacuum
%
≤10
GB/T17794-2008
Dimension stability
105±3°C,7d
%
≤10
GB/T8811
Crack resistance
N/cm
≥2.5
GB/T10808
Compression resilience ratio
Compression time 72h
%
≥70
GB/T6669-2001
Anti-ozone
Ozone pressure 202mpa
200h
——
Not cracking
GB/T7762
Aging resistance
150h
——
Slightly crumpling,
no cracks,
GB/T16259
Temperature
°C
-40°C——110°C
GB/T17794